Originally Posted by The_Bishop View Post
You could try Naval Jelly to remove the rust in the pits, then a good wash afterwards to neutralize, followed by the DX579/DX520. I'd contact PPG to make sure this will work well before priming. Epoxy primer?
Yeah, DP90LF. PPG's sheets list it as appropriate after the 579/520.

I may drag out one of the panels I'm scrapping and try the Naval Jelly on that.